- Made of 3.3 borosilicate glass
- Particularly adapted to analytical work where precipitates are dried to constant weight at 110°C
- In order to avoid strain, they should not be removed from the furnace until the temperature has dropped to 250°C
- Crucibles should not be subjected to sudden temperature change
Cat. No. |
Capacity mL |
Porosity Grade mm |
Dia. Of Disc mm |
Approx. Height mm |
Pore Size in µm |
Pack Size |
SW29000111 |
15 |
1 |
20 |
50 |
160-250 |
4 |
SW29000211 |
15 |
2 |
20 |
50 |
100-160 |
4 |
SW29000311 |
15 |
3 |
20 |
50 |
40-100 |
4 |
SW29000411 |
15 |
4 |
20 |
50 |
16-40 |
4 |
SW29000511 |
15 |
5 |
20 |
50 |
Oct-16 |
4 |
SW290001M1 |
30 |
1 |
30 |
60 |
160-250 |
4 |
SW290002M1 |
30 |
2 |
30 |
60 |
100-160 |
4 |
SW290003M1 |
30 |
3 |
30 |
60 |
40-100 |
4 |
SW290004M1 |
30 |
4 |
30 |
60 |
16-40 |
4 |
SW290005M1 |
30 |
5 |
30 |
60 |
Oct-16 |
4 |
SW29000125 |
50 |
1 |
40 |
65 |
160-250 |
4 |
SW29000225 |
50 |
2 |
40 |
65 |
100-160 |
4 |
SW29000325 |
50 |
3 |
40 |
65 |
40-100 |
4 |
SW29000425 |
50 |
4 |
40 |
65 |
16-40 |
4 |
SW29000525 |
50 |
5 |
40 |
65 |
Oct-16 |
4 |